Carácter del producto:
GH3536 high-temperature alloy is a nickel based alloy with high iron content that has been solid solution strengthened with Cr and Mo elements high temperature alloy, which has good corrosion resistance and oxidation resistance, can be used for a long time at 900 ℃, suitable for manufacturing combustion chamber components of aircraft engines with a short-term working temperature of 1080 ℃ other high-temperature components.
| Marca | Jinchun |
| Origen | China |
| Nombre del producto | GH3536 powder |
| Aplicación | Combustion chamber components of aircraft engines and other high-temperature components. |
| Forma | Polvo |
| Color | Metal gray |
| Talla | 15~53μm |
| Estándar | GB/T 19001-2016/ISO9001: 2015 |
| Pureza | Ni: Bal. Cr: 20.5-23.0%, Mo:8.0-10.0%, Co:0.5-2.5%,Fe: 17.0-20.0% |
| Material | Ni, Cr, Mo, Co, Fe |
| Embalaje | Envasado al vacío |
| Composición química (peso %) | |||||||||
| Elemento | C | Cr | Ni | Co | Mo | Al | Ti | Fe | B |
| Estándar | 0.05~0.15 | 20.5~23.0 | Bal. | 0.5~2.5 | 8.0~10.0 | ≤0.50 | ≤0.15 | 17.0~20.0 | ≤0.010 |
| typical | 0.08 | 21.94 | Bal. | 1.42 | 8.97 | 0.14 | 0.012 | 18.98 | 0.002 |
| Elemento | Mn | P | S | Cu | W | Si | O | N | |
| Estándar | ≤1.0 | ≤0.025 | ≤0.015 | ≤0.50 | 0.2-1.0 | ≤1.0 | ≤0.030 | ≤0.030 | |
| typical | 0.26 | 0.005 | 0.005 | 0.007 | 0.55 | 0.34 | 0.017 | 0.024 | |
| GH3536 | 15~53μm Distribución del tamaño de las partículas | Caudal (seg. para 50 g) | Densidad aparente (g/cm3) | Densidad del grifo (g/cm3) | ||
| D10 | D50 | D90 | ||||
| Estándar | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typical | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |
Imágenes de producción y pruebas: