Carácter del producto:
GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.
Marca | Jinchun |
Origen | China |
Nombre del producto | GH3625 powder |
Aplicación | Aviation engine components, aerospace structural components, and chemical equipment components. |
Forma | Polvo |
Color | Metal gray |
Talla | 15~53μm |
Estándar | GB/T 19001-2016/ISO9001: 2015 |
Pureza | Ni: Bal. Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15% |
Material | Ni, Cr, Mo, Nb |
Embalaje | Envasado al vacío |
Composición química (peso %) | ||||||||
Elemento | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
Estándar | ≤0.10 | 20.0~23.0 | Bal. | ≤1.0 | 8.0~10.0 | ≤0.40 | ≤0.40 | ≤5.0 |
typical | 0.0048 | 22.42 | Bal. | 0.006 | 9.12 | 0.13 | 0.018 | 0.72 |
Elemento | Mn | P | S | Cu | Nb | Si | O | N |
Estándar | ≤0.50 | ≤0.015 | ≤0.015 | ≤0.070 | 3.15~4.15 | ≤0.50 | ≤0.030 | ≤0.030 |
typical | 0.031 | 0.007 | 0.0014 | 0.011 | 3.75 | 0.025 | 0.014 | 0.013 |
GH3625 | 15~53μm Distribución del tamaño de las partículas | Caudal (seg. para 50 g) | Densidad aparente (g/cm3) | Densidad del grifo (g/cm3) | ||
D10 | D50 | D90 | ||||
Estándar | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
typical | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |