Caractéristiques du produit:
GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.
| Nom de la marque | Jinchun |
| Origine | Chine |
| Nom du produit | GH3625 powder |
| Application | Aviation engine components, aerospace structural components, and chemical equipment components. |
| Forme | Poudre |
| Couleur | Gris métal |
| Taille | 15~53μm |
| Standard | GB/T 19001-2016/ISO9001 : 2015 |
| La pureté | Ni: Bal. Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15% |
| Matériau | Ni, Cr, Mo, Nb |
| Emballage | Emballage sous vide |
| Composition chimique (wt.%) | ||||||||
| Élément | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
| Standard | ≤0.10 | 20.0~23.0 | Bal. | ≤1.0 | 8.0~10.0 | ≤0.40 | ≤0.40 | ≤5.0 |
| typique | 0.0048 | 22.42 | Bal. | 0.006 | 9.12 | 0.13 | 0.018 | 0.72 |
| Élément | Mn | P | S | Cu | Nb | Si | O | N |
| Standard | ≤0.50 | ≤0.015 | ≤0.015 | ≤0.070 | 3.15~4.15 | ≤0.50 | ≤0.030 | ≤0.030 |
| typique | 0.031 | 0.007 | 0.0014 | 0.011 | 3.75 | 0.025 | 0.014 | 0.013 |
| GH3625 | 15~53μm Distribution de la taille des particules | Débit (sec. pour 50 g) | Densité apparente (g/cm3) | Densité (g/cm3) | ||
| D10 | D50 | D90 | ||||
| Standard | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typique | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |
Photos de la production et des essais :




4.Application