Chengdu Jinchun Metallic Materials Co.,Ltd.

Spherical Metal Powders GH4169 Nickel based powder

Product Character:

GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

Brand Name Jinchun
Origin China
Product name GH4169 powder
Application Hot end structural components  in aerospace, energy, military and other fields.
Shape Powder
Color Metal gray
Size 15~53μm
Standard GB/T 19001-2016/ISO9001: 2015
Purity  Ni: 50-55%, Cr:17-21%, Mo:2.8-3.3%, Nb: 4.75-5.50%, Ti:0.65-1.15%, Fe: Bal.
Material Ni, Cr, Mo, Nb, Ti, Fe
Packing Vacuum packing
Product Character GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.   2.Specification GH4169 powder
Chemical  Composition (wt.%)
Element C Cr Ni Co Mo Al Ti Fe B
Standard ≤0.08 17.0~21.0 50.0~55.0 ≤1.0 2.8~3.3 0.2~0.8 0.65~1.15 Bal. ≤0.006
typical 0.078 18.97 52.98 0.005 3 0.65 1.1 Bal. 0.005
Element Mn P S Cu Mg Si Nb O N
Standard ≤0.35 ≤0.05 ≤0.015 ≤0.30 ≤0.01 ≤0.35 4.75~5.50 ≤0.030 ≤0.030
typical 0.33 0.009 0.0078 0.0039 0.002 0.32 5.02 0.017 0.01
 
GH4169 15~53μm Particle Size Distribution Flow Rate (sec. for 50 g) Apparent density  (g/cm3) Tap density  (g/cm3)
D10 D50 D90
Standard 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typical 22.3μm 34.9μm 53.3μm 17 4.22 4.93
  3.Pictures of Powder SEM morphology Pictures of Production and Test:   4.Application
  • GH4169  powder is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

5.Quality Assurance