Product Character:
GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.
| Brand Name | Jinchun |
| Origin | China |
| Product name | GH3625 powder |
| Application | Aviation engine components, aerospace structural components, and chemical equipment components. |
| Shape | Powder |
| Color | Metal gray |
| Size | 15~53μm |
| Standard | GB/T 19001-2016/ISO9001: 2015 |
| Purity | Ni: Bal. Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15% |
| Material | Ni, Cr, Mo, Nb |
| Packing | Vacuum packing |
| Chemical Composition (wt.%) | ||||||||
| Element | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
| Standard | ≤0.10 | 20.0~23.0 | Bal. | ≤1.0 | 8.0~10.0 | ≤0.40 | ≤0.40 | ≤5.0 |
| typical | 0.0048 | 22.42 | Bal. | 0.006 | 9.12 | 0.13 | 0.018 | 0.72 |
| Element | Mn | P | S | Cu | Nb | Si | O | N |
| Standard | ≤0.50 | ≤0.015 | ≤0.015 | ≤0.070 | 3.15~4.15 | ≤0.50 | ≤0.030 | ≤0.030 |
| typical | 0.031 | 0.007 | 0.0014 | 0.011 | 3.75 | 0.025 | 0.014 | 0.013 |
| GH3625 | 15~53μm Particle Size Distribution | Flow Rate (sec. for 50 g) | Apparent density (g/cm3) | Tap density (g/cm3) | ||
| D10 | D50 | D90 | ||||
| Standard | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typical | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |
Pictures of Production and Test: