Produktcharakter:
GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.
| Markenname | Jinchun |
| Herkunft | China |
| Name des Produkts | GH3625 powder |
| Anmeldung | Aviation engine components, aerospace structural components, and chemical equipment components. |
| Form | Pulver |
| Farbe | Metal gray |
| Größe | 15~53μm |
| Standard | GB/T 19001-2016/ISO9001: 2015 |
| Reinheit | Ni: Bal. Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15% |
| Material | Ni, Cr, Mo, Nb |
| Verpacken | Vakuumverpackung |
| Chemische Zusammensetzung (wt.%) | ||||||||
| Element | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
| Standard | ≤0.10 | 20.0~23.0 | Bal. | ≤1.0 | 8.0~10.0 | ≤0.40 | ≤0.40 | ≤5.0 |
| typisch | 0.0048 | 22.42 | Bal. | 0.006 | 9.12 | 0.13 | 0.018 | 0.72 |
| Element | Mn | P | S | Cu | Nb | Si | O | N |
| Standard | ≤0.50 | ≤0.015 | ≤0.015 | ≤0.070 | 3.15~4.15 | ≤0.50 | ≤0.030 | ≤0.030 |
| typisch | 0.031 | 0.007 | 0.0014 | 0.011 | 3.75 | 0.025 | 0.014 | 0.013 |
| GH3625 | 15~53μm Partikelgrößenverteilung | Durchflussrate (sec. für 50 g) | Scheinbare Dichte (g/cm3) | Klopfdichte (g/cm3) | ||
| D10 | D50 | D90 | ||||
| Standard | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typisch | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |
Bilder von Produktion und Test: