GH3536 high-temperature alloy is a nickel based alloy with high iron content that has been solid solution strengthened with Cr and Mo elements high temperature alloy, which has good corrosion resistance and oxidation resistance, can be used for a long time at 900 ℃, suitable for manufacturing combustion chamber components of aircraft engines with a short-term working temperature of 1080 ℃ other high-temperature components.
| 브랜드 이름 | 진춘 |
| 원산지 | 중국 |
| 제품 이름 | GH3536 powder |
| 애플리케이션 | Combustion chamber components of aircraft engines and other high-temperature components. |
| 모양 | 파우더 |
| 색상 | Metal gray |
| 크기 | 15~53μm |
| 표준 | GB/T 19001-2016/ISO9001: 2015 |
| 순도 | Ni: Bal. Cr: 20.5-23.0%, Mo:8.0-10.0%, Co:0.5-2.5%,Fe: 17.0-20.0% |
| 재료 | Ni, Cr, Mo, Co, Fe |
| 포장 | 진공 포장 |
| 화학 성분(중량 %) | |||||||||
| 요소 | C | Cr | Ni | Co | Mo | Al | Ti | Fe | B |
| 표준 | 0.05~0.15 | 20.5~23.0 | Bal. | 0.5~2.5 | 8.0~10.0 | ≤0.50 | ≤0.15 | 17.0~20.0 | ≤0.010 |
| typical | 0.08 | 21.94 | Bal. | 1.42 | 8.97 | 0.14 | 0.012 | 18.98 | 0.002 |
| 요소 | Mn | P | S | Cu | W | Si | O | N | |
| 표준 | ≤1.0 | ≤0.025 | ≤0.015 | ≤0.50 | 0.2-1.0 | ≤1.0 | ≤0.030 | ≤0.030 | |
| typical | 0.26 | 0.005 | 0.005 | 0.007 | 0.55 | 0.34 | 0.017 | 0.024 | |
| GH3536 | 15~53μm 입자 크기 분포 | 유량 (50g의 경우 초) | 겉보기 밀도(g/cm3) | 탭 밀도(g/cm3) | ||
| D10 | D50 | D90 | ||||
| 표준 | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typical | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |