구형 금속 분말 GH4169 니켈 기반 분말

제품 캐릭터 : 제품 캐릭터

GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

브랜드 이름 진춘
원산지 중국
제품 이름 GH4169 powder
애플리케이션 Hot end structural components  in aerospace, energy, military and other fields.
모양 파우더
색상 Metal gray
크기 15~53μm
표준 GB/T 19001-2016/ISO9001: 2015
순도  Ni: 50-55%, Cr:17-21%, Mo:2.8-3.3%, Nb: 4.75-5.50%, Ti:0.65-1.15%, Fe: Bal.
재료 Ni, Cr, Mo, Nb, Ti, Fe
포장 진공 포장
제품 캐릭터 GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.   2.사양 GH4169 powder
화학 성분(중량 %)
요소 C Cr Ni Co Mo Al Ti Fe B
표준 ≤0.08 17.0~21.0 50.0~55.0 ≤1.0 2.8~3.3 0.2~0.8 0.65~1.15 Bal. ≤0.006
typical 0.078 18.97 52.98 0.005 3 0.65 1.1 Bal. 0.005
요소 Mn P S Cu Mg Si Nb O N
표준 ≤0.35 ≤0.05 ≤0.015 ≤0.30 ≤0.01 ≤0.35 4.75~5.50 ≤0.030 ≤0.030
typical 0.33 0.009 0.0078 0.0039 0.002 0.32 5.02 0.017 0.01
 
GH4169 15~53μm 입자 크기 분포 유량 (50g의 경우 초) 겉보기 밀도(g/cm3) 탭 밀도(g/cm3)
D10 D50 D90
표준 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typical 22.3μm 34.9μm 53.3μm 17 4.22 4.93
  3. 분말 SEM 형태 사진 프로덕션 및 테스트 사진:   4.애플리케이션
  • GH4169  powder is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.