Spherical Metal Powders GH3625 Superalloy High-temperature alloy Powder

Carácter do produto:

GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.

Nome da marca Jinchun
Origem China
Nome do produto GH3625 powder
Aplicação Aviation engine components, aerospace structural components, and chemical equipment components.
Forma
Cor Metal gray
Tamanho 15~53μm
Padrão GB/T 19001-2016/ISO9001: 2015
Pureza  Ni: Bal.  Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15%
Material Ni, Cr, Mo, Nb
Embalagem Embalagem a vácuo
Carácter do produto GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.   2.Especificação GH3625 powder
Composição química (wt.%)
Elemento C Cr Ni Co Mo Al Ti Fe
Padrão ≤0.10 20.0~23.0 Bal. ≤1.0 8.0~10.0 ≤0.40 ≤0.40 ≤5.0
typical 0.0048 22.42 Bal. 0.006 9.12 0.13 0.018 0.72
Elemento Mn P S Cu Nb Si O N
Padrão ≤0.50 ≤0.015 ≤0.015 ≤0.070 3.15~4.15 ≤0.50 ≤0.030 ≤0.030
typical 0.031 0.007 0.0014 0.011 3.75 0.025 0.014 0.013
 
GH3625 15~53μm Distribuição do tamanho das partículas Caudal (seg. para 50 g) Densidade aparente (g/cm3) Densidade da torneira (g/cm3)
D10 D50 D90
Padrão 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typical 23.4μm 36.2μm 55.2μm 20 4.24 5.03
  3. imagens da morfologia SEM do pó Fotos de produção e teste:   4.Aplicação
  • GH3625  powder  is applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.