Carácter do produto:
GH3625 high-temperature alloy belongs to solid solution strengthening alloys with added elements such as Nb, Mo, Cr, etc., and has high strength, excellent corrosion resistance and oxidation resistance, and resistance to stress corrosion under salt spray atmosphere applied in the manufacturing of aviation engine components, aerospace structural components, and chemical equipment components.
| Nome da marca | Jinchun |
| Origem | China |
| Nome do produto | GH3625 powder |
| Aplicação | Aviation engine components, aerospace structural components, and chemical equipment components. |
| Forma | Pó |
| Cor | Metal gray |
| Tamanho | 15~53μm |
| Padrão | GB/T 19001-2016/ISO9001: 2015 |
| Pureza | Ni: Bal. Cr: 20.0-23.0%, Mo:8.0-10.0%, Nb: 3.15-4.15% |
| Material | Ni, Cr, Mo, Nb |
| Embalagem | Embalagem a vácuo |
| Composição química (wt.%) | ||||||||
| Elemento | C | Cr | Ni | Co | Mo | Al | Ti | Fe |
| Padrão | ≤0.10 | 20.0~23.0 | Bal. | ≤1.0 | 8.0~10.0 | ≤0.40 | ≤0.40 | ≤5.0 |
| typical | 0.0048 | 22.42 | Bal. | 0.006 | 9.12 | 0.13 | 0.018 | 0.72 |
| Elemento | Mn | P | S | Cu | Nb | Si | O | N |
| Padrão | ≤0.50 | ≤0.015 | ≤0.015 | ≤0.070 | 3.15~4.15 | ≤0.50 | ≤0.030 | ≤0.030 |
| typical | 0.031 | 0.007 | 0.0014 | 0.011 | 3.75 | 0.025 | 0.014 | 0.013 |
| GH3625 | 15~53μm Distribuição do tamanho das partículas | Caudal (seg. para 50 g) | Densidade aparente (g/cm3) | Densidade da torneira (g/cm3) | ||
| D10 | D50 | D90 | ||||
| Padrão | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
| typical | 23.4μm | 36.2μm | 55.2μm | 20 | 4.24 | 5.03 |